Propiedades | Método de ensayo | Unidad | El promedio mínimo de valor | ||||
MWG270 | MWG370 | MWG570 | MWG665 | MWG770 | |||
Fuerza tensil , MD | La norma ASTM D 4595 | KN/m | 38.5 | 52.5 | 70 | 70 | 105.1 |
Fuerza tensil , CD | La norma ASTM D 4595 | KN/m | El 35,9 | 47.3 | 70 | El 96,3 | 84 |
La elongación, MD | La norma ASTM D 4595 | % | 25 | 25 | 25 | 25 | 25 |
La elongación, CD | La norma ASTM D 4595 | % | 25 | 25 | 25 | 25 | 25 |
Resistencia en | |||||||
El 2%, MD | La norma ASTM D 4595 | KN/m | 7 | 11 | 14 | 17.5 | 21 |
El 2%, CD | La norma ASTM D 4595 | KN/m | 8.6 | 12.3 | 19.3 | 25 | 22.8 |
El 5%, MD | La norma ASTM D 4595 | KN/m | 17.7 | 21.9 | 35 | 35 | 52.5 |
El 5%, CD | La norma ASTM D 4595 | KN/m | 19.8 | 22.8 | 39.4 | 53 | 47.1 |
La fábrica de costura de la fuerza | La norma ASTM D 4884 | KN/m | 18.4 | 25.1 | 37.5 | 52.5 | 43.8 |
Tamaño de abertura aparente | La norma ASTM D 4751 | Mm | 0.6 | 0.43 | 0.6 | 0.43 | 0.6 |
Permitividad | La norma ASTM D 4491 | S-1 | 0.7 | 0.9 | 0.4 | 0.26 | 0.04 |
Caudal de agua | La norma ASTM D 4491 | L/min/m2 | 2037 | 1630 | 1222 | 815 | 611 |
Resistencia UV (% retenido después de 500 horas). | La norma ASTM D 4355 | % | 80 | 80 | 80 | 70 | 80 |