Lama per sega a freddo Cermet 285mm-72 per il taglio di metalli

Model No.
285*32*72
Tipo
HSS Lama
nome
lama circolare per sega cermet
personalizzato
personalizzato
applicazione di taglio
tubi in acciaio al carbonio,acciaio inox,lega di titanio,
attrezzature adatte
macchine a sega circolare ad alta velocità
Pacchetto di Trasporto
Cartons/Pallets
Specifiche
285/300/315/330/360/380/400/425/460/485/520/560
Marchio
Hante
Origine
Made in China
Codice SA
8202301000
Capacità di Produzione
600000pieces/Year
Prezzo di riferimento
$ 85.50 - 94.50

Descrizione del Prodotto

  Our ceramic carbide cold saw blades the  are designed for work-piece materials: steek,iron,aluminum,copper,especially for stainless steel,hardened steel,titanium alloy,PCB(print circuit board).Too life of the solid carbide saw blades is 6-7 times
more than the ones of HSS(High speed steel),perfect surface of solid carbide saw blades for high precision,which is the optimized option to replace the HSS saw blades.

 
saw blade Basic information
saw blade brand Hante blade material alloy
blade brand Sandvik blade  origin Germany
base material SK 8 Tool steel basic brand new Nippon iron  ( Nippon steel)
base origin Japan Coating material titanium silicon
suitable material 304, 306, 316 stainless steel, titanium alloy and other hard materials

Sawing parameters
Sawing material Steel grade Material characteristics Material diameter recommended saw blade specifications Select type saw blade speed(RPM) Feed speed (mm/s) feed amount (wire/tooth )feed * 60 + speed + number of teeth
stainless steel 304 The material is sticky and has high hardness ∅30-70 ∅285*60T/72T 70/75 60-75 2.5-4 3-4.5
stainless steel 316 The material is sticky and has high hardness ∅30-90 ∅300*60T/72T 80/90 60-75 2.5-4 3-4.5
∅315*60T/72T

 
Saw blade use precautions
1. The saw blade must be installed correctly when installing, check several times more, incorrect installation will affect the surface quality of saw-cutting products, but also affect the life of saw blade.
2,The cleaning of circular sawing machine is not in place, especially if there are iron chips in it can cause the saw blade to consume too quickly.
3,The saw blade should be handled gently to avoid bumping into the surface of the saw blade. The surface of the saw blade is not smooth and the friction force increases.
4,Cutting parameters are related to cutting materials. Different materials should choose different cutting parameters, and cutting efficiency can not be pursued to lead to the fatigue of the saw blade in advance.
5,Before cutting materials, pay attention to clean the oxide scale and iron chips on the surface of the material to avoid large friction and excessive loss of the saw blade.
6,The equipment works for a long time, the saw blade load is increased, can not be buffered, loss too fast is inevitable.

285mm-72 Cermet Cold Saw Blade for Metal Cutting

285mm-72 Cermet Cold Saw Blade for Metal Cutting

285mm-72 Cermet Cold Saw Blade for Metal Cutting

285mm-72 Cermet Cold Saw Blade for Metal Cutting


285mm-72 Cermet Cold Saw Blade for Metal Cutting
285mm-72 Cermet Cold Saw Blade for Metal Cutting




 

La Lama Della Sega

TREF.COM.MK, 2023